www.pcimag.com/articles/86240-air-products-and-chemicals-air-products-polymers-l-p-business
Air Products and Chemicals: Air Products Polymers L.P. business
December 22, 2000
Air Products and Chemicals said its Air Products Polymers L.P. business formally dedicated a new exterior testing facility designed to evaluate the exterior durability of products formulated with the company’s resins and additives for architectural and industrial-maintenance coatings.
Air Products and Chemicals Inc., Lehigh Valley, PA, said its Air Products Polymers L.P. business formally dedicated a new exterior testing facility designed to evaluate the exterior durability of products formulated with the company’s resins and additives for architectural and industrial-maintenance coatings. The company said the site, at Trexlertown, PA, enhances its research capabilities, development of new products, and investigation of existing problems in customer products. The facility allows exposure of coated panels on a variety of substrates, with exposures carried out at a variety of angles.
Air Products and Chemicals Inc., Lehigh Valley, PA, said its Air Products Polymers L.P. business formally dedicated a new exterior testing facility designed to evaluate the exterior durability of products formulated with the company’s resins and additives for architectural and industrial-maintenance coatings. The company said the site, at Trexlertown, PA, enhances its research capabilities, development of new products, and investigation of existing problems in customer products. The facility allows exposure of coated panels on a variety of substrates, with exposures carried out at a variety of angles.