HunterLab: Color-Measurement System
June 1, 2000
The ColorFlex™ is a small, benchtop, self-contained color-measurement spectrophotometer. Its rugged design and small size allow users to measure the color of raw material and final product in locations throughout the production facility. Data can be stored in the instrument and printed out on a standard printer. The instrument can be connected to a PC and used with the company’s Universal® quality-control software.