Shipping sacks made with ValeronĀ® strength film can replace thicker gauged multi-wall and low-grade polymer sacks by offering high burst strength, tear resistance and high puncture resistance. The film can be used in shipping sacks for the chemical, export, photographic, and lawn and garden chemical packaging.