High-Temperature Paint Helps Solve Lighting Problems at Major Sports Arenas
Paint-Line, Inc., Fairfield, Iowa, specializes in applying high-temperature paints to lighting fixtures for the entertainment and sports industries. Racing speedways and sports venues are equipped with long-lasting and reliable outdoor permanent lighting fixtures coated by Paint-Line.
Frank Nelson, operations manager at Paint-Line, reports that they apply a specially formulated high-temperature Pyromark® coating from Tempil, an ITW company, South Plainfield, NJ, to protect lighting fixtures and assure their long-term performance.
The Pyromark paint is specially formulated for protecting, decorating or color identifying metal surfaces that will be subjected to high temperatures. They are silicon-based coatings that provide long-lasting protection against oxidation and corrosion, and offer excellent covering characteristics. They will not blister, chip, crack or peel at their rated temperature. Their solar absorptivity of 0.95 makes them an almost perfect black box absorber.
Pyromark 1200 flat black paint is sprayed on with a high-volume, low-pressure (HVLP) gun. Once applied, Nelson adds, "The silicone coating must withstand high wattage and temperatures, sometimes up to 2,000 ºF. It provides long-lasting protection against oxidation and corrosion because of its extraordinary absorptivity and emissivity properties up to 2,000 ºF. Pyromark's excellent covering characteristics prevent blistering, chipping, cracking or peeling", he explains.

Controlled vitrification is the key to the very high-temperature service capability of the coatings. In effect, vitrification converts silicone resins to inorganic silica, producing a thin but tenacious refractory coating, which will withstand higher temperatures than most conventional coatings. Tempil reports that Pyromark has been used for applications that include infrared heaters, boilers, furnaces, fireplace accessories, solar absorbers, stoves, and boat and auto engines or any other metal surfaces that are subject to high temperatures.
Pyromark is available in three varieties to coat metal surfaces that will be exposed to high temperatures: Series 800, Series 1200 and Series 2500.