www.pcimag.com/articles/84561-company-news-futura-coatings-1

Company News: Futura Coatings

September 26, 2000
Futura Coatings announced that its European subsidiary, Futura Tech International, has moved into new office and warehouse facilities in Menen, Belgium.

Futura Coatings Inc., St. Louis, announced that its European subsidiary, Futura Tech International, has moved into new office and warehouse facilities in Menen, Belgium. The St. Louis-based company also has named Guy Vanoosthuyse operations manager for Futura Tech, with responsibility for day-to-day business and customer-service operations. Futura President Rodney Jarboe said the moves are part of the company’s efforts to better serve the shipping and technical-service needs of European customers. Futura is a manufacturer of polyurethane and polyurea coatings, binders, elastomers, and structural resins.