UCB Chemicals Corp.’s Powder Resins Business Unit introduces Crylcoat® 310. The hybrid resin is a carboxyl terminated polyester resin designed for use with epoxy resins, and cure in temperatures of 160ºC or 320ºF. It combines good flow and flexibility, and high gloss.