www.pcimag.com/articles/82874-bohlin-instruments-rheometer

Bohlin Instruments: rheometer

July 25, 2000
The new CVO120 rheometer can measure the mechanical properties of solids and films across a range of temperatures. The instrument uses a DMTA cell that allows full-length solids and delicate films to be easily mounted in specially designed test clamps. Windows software enables temperature gradients to be preprogrammed over the range –150ºC to 550ºC.