Image courtesy of Wall Colmonoy Corporation.
Wall Colmonoy Launches Advanced Tungsten Carbide Powders for Thermal Spray Applications
Wall Colmonoy Corporation, a global leader in surfacing, brazing, and engineered materials, announced the launch of its WallCarb™ HVOF Tungsten Carbide Powders.
Designed for thermal spray applications, WallCarb™ HVOF Carbide Powders provide dense, hard coatings with exceptional wear and corrosion resistance. Their spherical, spray-dried, and sintered design ensures high deposit efficiency and consistent application parameters. The result is a smooth coating with minimal porosity, reducing the need for extensive finishing and grinding while improving overall process efficiency.
WallCarb™ HVOF Powders are ideal for industries such as oil and gas, mining, steel, and power generation. Available options include:
- WallCarb™ 86/10/4 – WC10Co4Cr
- WallCarb™ 90/10 – WC10Ni
- WallCarb™ 73/20/7 – WC20Cr7Ni
- WallCarb™ 88/12 – WC12Co
- WallCarb™ 75/25 – Cr3C2 25 (80Ni 20Cr)
WallCarb™ HVOF Powders are offered in 5 kg bottles in particle size distributions of -45+15 µm or -38+10 µm, formulated for various HVOF systems. Additional grades and particle size distributions are available upon request.
This launch reinforces Wall Colmonoy’s commitment to delivering industry-leading engineered materials that meet the demands of high-performance industrial applications.
For more information, visit wallcolmonoy.com/wallcarb-powders.