CRX Coatings Launches Graphene-Enhanced Marine Paint
November 13, 2024
CRX Coatings has introduced a graphene-infused bottom paint for the boating industry, designed to enhance hull protection and performance. The innovative formula leverages graphene’s properties to improve durability and reduce maintenance requirements. This development represents a significant advancement in marine coatings, offering boat owners a new option for hull maintenance.