Removable Coating for the Most Corrosive Conditions

April 16, 2024

VpCI®-368 is a solvent-based, temporary wax-like coating that provides protection in harsh, unsheltered environments. It dries quickly to a slightly brown finish and protects at 2-3 mils (50-75 µm) DFT (dry film thickness). It can be removed with an alkaline cleaner or flash rust inhibiting cleaner. VpCI®-368 can be applied to new equipment in transit or use equipment that needs to be laid up, for applications such as rig stacking or other large preservation projects. It is often the default coating for stationary surfaces.