www.pcimag.com/articles/110271-anti-abrasive-graphene-enhanced-architectural-paint-from-gerdau-graphene
ArchitecturalCoatings-126260819.jpg

Anti-Abrasive, Graphene-Enhanced Architectural Paint from Gerdau Graphene

July 5, 2022

SÃO PAULO — Gerdau Graphene, a nanotechnology company pioneering advanced graphene-enhanced materials for industrial applications, has created a new water-based architectural paint that is reported to be significantly more durable and resistant to abrasion than traditional paints. The new paint is ideal for use on concrete, cement, metal and asphalt, such as on sidewalks, bicycle lanes, garages, staircases, sports courts, and a wide array of commercial and industrial areas. Its parent company, Gerdau, began applying the new paint to its factory floors in March, reportedly making it the world’s first large-scale use of a water-based graphene-enhanced architectural paint. The company is already selling its proprietary graphene additives as development prototypes to major paint producers in the Americas. The announcement follows recent news that the company has developed new graphene-enhanced thermoplastics.

“This new graphene-based floor paint is extremely abrasion-resistant and requires less maintenance and repainting over its lifetime compared with traditional paints. Based on the performance gains of our new product, it’s clear that graphene will have a transformational impact on the entire paint industry,” said Alexandre Corrêa, CEO of Gerdau Graphene. “We are proud to have painted our specialty steel plant in São Paulo in March and have since moved to paint all our assets in Brazil in the coming months. In addition, we have commercialized this new paint for key clients and partners in the construction industry to paint industrial, commercial, and residential building floors. We will continue to optimize our additives to meet the needs of customers and scale commercialization of these paint products globally.”

The development of the graphene-based paint started in December 2021 and is the result of a partnership with Grafftex, a Brazilian paint manufacturer, and Polystell, a company focused on research and development of chemical additives. Gerdau Graphene created the graphene technology used to disperse graphene into a paint additive. Because graphene comes in a variety of types and shapes, each of which has unique properties, significant research and testing was required to determine the best graphene format needed to produce a superior paint product. In addition, graphene additives need to be customized based on each paint manufacturer’s unique formula and ingredients.

Gerdau Graphene is also working on additives for anti-corrosion paints, focusing on reducing heavy metals and fossil-based ingredients from light and heavy maintenance paints. The company reports that in 2020, U.S. architectural paint consumption was approximately 850 million gallons, or roughly 60% of the total 1.4 billion gallons of paint sold. The U.S. architectural paint market size is expected to cross $15 billion by 2025. “Our plan is to pilot this coating in our own operations and then launch the new products commercially in early 2023,” said Corrêa.

Gerdau Graphene is a nanotech company focused on the production, development and commercialization of graphene-enhanced products including polymers, paints and coatings, rubber, and more. To learn more, visit gerdaugraphene.com.