HOUSTON – OQ Chemicals announced the company has increased prices for the certain products. The increase became effective June 1, 2022, or as contracts allow.
In North America and Mexico, n-butyl acetate, isobutyl acetate and n-propyl acetate increased $0.10/lb. In South America, n-butyl acetate, isobutyl acetate and n-propyl acetate increased $220/mt.