EPS Features High-Value Acrylic Resins and Colorants
Engineered Polymer Solutions® (EPS®) is showcasing its line of high-value, sustainable products for the construction, industrial and architectural coatings industries at Booth 2364.
EPS will highlight this broad range of innovative products at the show:
· EPS® 2252: A high solids, all-acrylic polymer with exceptional adhesion to TPO, EPDM, metal, asphalt and other common roofing substrates that allows coatings to be formulated at <50 g/L VOC.
· EPS® 2580: A direct-to-metal polymer that offers exceptional corrosion resistance, early water resistance and rapid hardness development. EPS 2580 can also be formulated at <50 g/L VOC.
· EPS® 2799: An all-acrylic, film-forming polymer that is an exceptional choice for high-performance gloss for interior and exterior architectural DIY or professional paints. Ideal for institutional, commercial or other high-traffic area wall coatings, EPS 2799 can be used to formulate near-zero-VOC paints using the EPS® 9147 coalescent.
· NovoColor® SF: A waterborne dispersion designed for the tinting of waterborne coatings and stains, especially wood stains, and other applications where a high degree of color transparency is desired.
“Our team of R&D experts is consistently thinking about the future, working on formulating next-generation products for the coatings industry,” says Jose Luna, Global Marketing Director, EPS. “For example, the acrylic resins we're highlighting at ACS can be used for low VOC formulations – helping our customers meet stringent regulatory standards while also exceeding performance requirements.”