BERKELEY, CA — Keyland Polymer and polySpectra recently announced a strategic partnership to provide UVMax powder coatings to COR Alpha 3D printed parts. This collaboration unlocks a new modular approach to additive manufacturing, enabling the direct digital fabrication of end-use polymer components for a wide variety of applications.

"The promise of 3D printing has always been to help innovators to quickly and efficiently make their ideas real," said polySpectra founder and CEO Raymond Weitekamp. "For 3D printing to make the transition into true production-grade additive manufacturing, designers, inventors and engineers need to be able to trust that their printed parts will have the accuracy, aesthetics and durability required to use in their application. We are now making good on that promise."

The surface color and texture of the UVMax coating can be tailored to make COR Alpha 3D printed parts indistinguishable from traditionally-manufactured polymer products. The color-matching capabilities of Keyland, combined with the versatility of polySpectra's Cyclic Olefin Resin (COR) family of materials, now enable consumer and industrial brands to adopt a completely new approach to digital manufacturing. Factors that make this partnership so unique include:

  • COR is the core – polySpectra's family of engineering-grade photopolymers unlock a diverse array of previously impossible additive manufacturing applications. For more than five years, the polySpectra team has been collaborating with end-users of 3D printing to refine COR Alpha for applications that require best-in-class thermomechanical performance and durability. From consumer products to medical devices to satellite parts, COR Alpha helps product teams accelerate innovation with advanced additive manufacturing.
  • UVMax coating provides a spectrum of color possibilities – Keyland's UVMax provides an excellent finish for plastic applications in transportation, light-weighting, building materials, consumer and industrial products. Keyland can develop a wide range of powders to match any supplied color standard. UV powder is an environmentally friendly coating, containing no solvents, VOCs or HAPs. It is safe to use and can be reclaimed and recycled.
  • Improved durability: inside and out – Both COR Alpha and UVMax were designed for durability. The high working temperature, toughness, and extreme chemical resistance of COR Alpha is enhanced by the hardness, abrasion resistance, and excellent adhesion of the UVMax coating. 

"We have spent years searching for a scalable & durable coating solution that would enable our customers to apply their favorite brand colors to COR Alpha parts," said Weitekamp. "With UVMax, we finally found the solution."

"Typical additive manufacturing polymers are challenging to coat. The high thermal stability of COR Alpha allows for a thorough and complete coating without the concern of warping or degrading the material," said Andrew S. Walton, Business Development Manager at Keyland Polymer.