July 1, 2021

The FRITSCH variable-speed rotor mill PULVERISETTE 14 classic line is ideal for the comminution of difficult-to-grind samples like temperature-sensitive powder coatings and plastic samples due to the line’s efficient air cooling and cyclone separators. An automatic speed compensation feature ensures an ideal adaptation of the grinding to the specific comminution behavior of the sample. Air routing ensures a constant airflow to cool the grinding material, and a fan blows the air into the instrument through a foam particle filter, creating positive pressure to prevent penetration of dirt particles from the ambient air. LEARN MORE