Graphene Nanotube Concentrates from OCSiAl Group
April 1, 2021
Recently developed graphene nanotube (single wall carbon nanotube) concentrates for powder coating formulations have expanded a line of nanotube products to all types of epoxy formulations. Just 0.2% wt. of a nanotube concentrate enables surface resistivity of 106 Ω/sq, but preserves color, surface quality, and rheological and mechanical performance of epoxy resin. Graphene nanotubes are used to produce high-performance epoxy coatings for aerospace, transportation, oil and gas, construction, electronics production, green technologies and other industries.