DOWSIL™ 211S additive is a low-cyclic, ultra-high molecular weight silicone delivered in a waterborne system that enhances mar resistance, slip and block resistance performance, enabling more durable, longer-lasting wood coatings. DOWSIL 107F additive is a low-cyclic silicone foam control agent with high effectiveness in waterborne acrylic clear wood coating varnishes, and acrylic, styrene acrylic and VAE emulsion paint for architectural wall coatings. DOWSIL 402LS additive is a silicone additive that reduces the coefficient of friction of wood coatings, and offers blocking resistance while improving flow and leveling properties.