World-Class Track and Field Facility Showcases Structural Wood Systems and Finishes

The Sansin Corporation, a global leader in environmentally friendly, high-performance wood protection, and Western Archrib, a leader in the design, manufacture and custom fabrication of glued-laminated (glulam) structural wood systems, announced today their products are showcased on the stunning track and field facility, Hayward Field, at the University of Oregon in Eugene.
The open and airy structure is funded by gifts from Penny and Phil Knight and more than 50 other donors. The world-class facility gives athletes an unparalleled stage for competition and training, and provides fans with a theater for track and field.
The newly reconstructed stadium, designed by SRG Partnership and constructed by Hoffman Construction, offers unobstructed views from all 12,650 seats. Elements of Historic Hayward Field, where Phil Knight competed in track and field events while attending the university, were incorporated into the new facility, preserving the rich heritage of the original stadium.
One of the main design objectives was to showcase Oregon history, culture and forest products. To that end, more than 462 Douglas Fir glulam structural wood pieces, sourced by Western Archrib and protected with Sansin’s low-VOC architectural finishes, were used to create 77 unique curves, each containing six pieces of curved wood. There were over one million linear feet of Douglas Fir lumber used in all the glulam pieces – equating to 830.5 laps around a 400-meter track. In fact, if the boards were laid end-to-end, they would stretch from Hayward Field to Oregon’s largest city of Portland and back again.
“This is an incredible mass timber structure,” said Mark Wigston, Senior Manager of Projects and Technical Services at Western Archrib. “It was a massive undertaking, starting with detailed and solution-minded team collaboration with the design group and trade partners. With the plan from the design group, we effectively and efficiently created 462 unique glulam members that are seamlessly integrated and showcased throughout the stadium canopy. This ultimately ensured we exceeded the vision and high expectations set by the design group. We were thrilled to partner with Sansin to provide the stunning glulam members for the project. By applying two coats of the Sansin finish in our shop prior to shipment, we were able to ensure the glulam members were protected in transit and in situ during construction.”
A three-coat KP-12UVW and Precision Coat ENS system in a custom tint were selected for their durability, beauty and environmental profile. The final coat of Precision Coat ENS was applied on the job site during construction.
“We are proud to be part of this iconic project,” said Caroline March-Long, Director of Sales and Marketing at Sansin. “We worked with the architectural team to develop a coating system that would bring out the character of the glulam pieces, while providing maintainable protection from UV and moisture.”
By the Numbers - Glulam Facts for Hayward Field Project
-
154 unique glulam curves
-
462 total number of glulam pieces
-
Deepest beam is 6’-9”; longest beam is 55’-10”
-
1,900,000 pounds of glulam weight
-
1,417 metric tons of carbon dioxide stored
-
1,966 metric tons of total carbon benefit – the equivalent of 416 cars being off the road for a year
To learn more, visit www.sansin.com.