Antiviral Wood Coating from Kubilay Boya
January 12, 2021
Kubilay Ultra Hygiene was tested against human coronavirus NL63, widely used as a model for SARS-CoV-2, and showed more than 90% virucidal activity according to ISO 21702 standard. Antibacterial and antifungal activity tests showed 99.99% antibacterial activity against several bacteria. Applications include furniture, public transport and airports. Learn more.