MACOMB, MI – Allied PhotoChemical has improved its R&D capabilities with the installation of a new Q-Fog CRH Cyclic Corrosion Tester, which provides new advanced features to help produce the best UV coatings for customers.

Cyclic corrosion testing provides the best possible laboratory simulation of natural atmospheric corrosion. The Q-Fog CRH Cyclic Corrosion Tester has the capabilities to control the volume of spray on specimens, giving more control of the distance and distribution of the corrosive solution, faster temperature adjusting, and a larger reservoir for extended continual testing.

Allied PhotoChemical is a leading formulator and producer of UV, solvent- and water-based coating technologies. Contact Allied at info@alliedphotochemical.com for more information.