Bisphenol Monomer from Songwon
May 1, 2020
BP-Z improves the mechanical proper-ties and heat resistance of specialty polycarbonate and polyester resins. Composed mainly of epoxy, phenolic and novolac resins, it is suitable for high-frequency, copper-clad laminates and electronic packaging. Visit songwon.com.