www.pcimag.com/articles/107386-roof-coating-resins-from-engineered-polymer-solutions

Roof Coating Resins from Engineered Polymer Solutions
May 1, 2020
EPSĀ® 2719 is an all-acrylic emulsion that minimizes asphalt bleed-through in cool roof coatings. It provides excel-lent adhesion to asphaltic and other construction substrates, and exceptional UV and dirt pickup resistance. EPS 2252 is a high-solids acrylic emulsion designed to adhere to low-energy substrates commonly used in roofing. Visit eps-materials.com.