www.pcimag.com/articles/107273-specialty-epoxy-resins-from-cvc-thermoset-specialties

Specialty Epoxy Resins from CVC Thermoset Specialties
April 1, 2020
HyPox CTBN-modified epoxy resins improve cathodic disbondment and toughness properties at various temperatures when used in girth weld and in FBE coatings. Call 856/533.7699.