Covestro Partners in Research Project to Develop Coatings for Wind Energy
LEVERKUSEN, Germany — One important hurdle on the path to achieving maintenance-free systems in the wind energy sector is the fact that the longitudinal edges of rotor blades are subject to the effects of weather: when it is raining and the blades are turning quickly, raindrops hit the edges of the blades at high speed and with a large amount of energy. Over time, this destroys the coating layer and the composite material beneath. This edge erosion can reduce annual energy performance by more than five percent. In addition, the systems have to be serviced more frequently.
A consortium managed by the Technical University of Denmark – the world’s largest public research institute focused on wind energy – is currently carrying out a research project named DURALEDGE (from Durable Leading Edges) to investigate erosion mechanisms and develop new coatings to permanently protect rotor blades. In addition, the consortium aims to develop calculation models to predict edge protection. Leading global manufacturers of wind energy systems and coatings are members of the consortium, as is Covestro as a key raw materials partner. The company has been engaged for many years in a sustainable energy supply.
“We are working at high speed to develop a raw material for a specialized, robust paint system,” said Dr. Matthias Wintermantel, Head of Market and Business Development Infrastructure Coatings at Covestro. “It will significantly increase the service life of rotor blades, while also reducing maintenance expenses and associated costs. This lets us help make sustainable energy production using wind power even more economical”.
One goal in developing future rotor blades is to increase the peak speed at the ends of the blades. The aim is an increase to over 90 meters per second to improve the performance of wind energy systems. This also lowers electricity generation costs for converting wind energy into electrical energy.
The DURALEDGE project started on Nov. 1, 2018, and has a term of three years. It is being funded with 11.7 million Danish Krones (around €1.57 million) from the Danish Innovation Fund.