Epoxy Resin from Sun Chemical

April 1, 2019

EPICLON® HP 4770 is a multi-functional naphthalene epoxy resin for formulators in the aerospace, transportation and electronics industries who seek to increase high-temperature performance. It provides high modulus/stiffness, low water absorption, improved mechanical properties, adhesion and good fiber wet out. Visit www.sunchemical.com/product/epiclonforaerospace.