Researchers Create ‘Smart’ Material With Antifouling Potential

February 28, 2019

PROVIDENCE, RI – Brown University researchers have shown a way to use graphene oxide (GO) to add some backbone to hydrogel materials made from alginate, a natural material derived from seaweed that’s currently used in a variety of biomedical applications. In a paper published in the journal Carbon, the researchers describe a 3-D printing method for making intricate and durable alginate-GO structures that are far stiffer and more fracture resistant that alginate alone.

“One limiting factor in the use of alginate hydrogels is that they’re very fragile — they tend to fall apart under mechanical load or in low salt solutions,” said Thomas Valentin, a Ph.D. student in Brown’s School of Engineering who led the work. “What we showed is by including graphene oxide nanosheets, we can make these structures much more robust.”

The material is also capable of becoming stiffer or softer in response to different chemical treatments, meaning it could be used to make “smart” materials that are able to react to their surroundings in real time, the research shows. In addition, alginate-GO retains alginate’s ability to repel oils, giving the new material potential as a sturdy antifouling coating.

The 3-D printing method used to make the materials is known as stereolithography. The technique uses an ultraviolet laser controlled by a computer-aided design system to trace patterns across the surface of a photoactive polymer solution. The light causes the polymers to link together, forming solid 3-D structures from the solution. The tracing process is repeated until an entire object is built layer-by-layer from the bottom up. In this case, the polymer solution was made using sodium alginate mixed with sheets of graphene oxide, a carbon-based material that forms one-atom-thick nanosheets that are stronger pound-for-pound than steel.

One advantage to the technique is that the sodium alginate polymers link through ionic bonds. The bonds are strong enough to hold the material together, but they can be broken by certain chemical treatments. That gives the material the ability to respond dynamically to external stimuli. Previously, the Brown researchers showed that this “ionic crosslinking” can be used to create alginate materials that degrade on demand, rapidly dissolving when treated with a chemical that sweeps away ions from the material’s internal structure.

For this new study, the researchers wanted to see how graphene oxide might change mechanical properties of alginate structures. They showed that alginate-GO could be made twice as stiff as alginate alone, and far more resistant to failure through cracking.

“The addition of graphene oxide stabilizes the alginate hydrogel with hydrogen bonding,” said Ian Y. Wong, an Assistant Professor of Engineering at Brown and the paper’s senior author. “We think the fracture resistance is due to cracks having to detour around the interspersed graphene sheets rather than being able to break right though homogeneous alginate.”

The extra stiffness enabled the researchers to print structures that had overhanging parts, which would have been impossible using alginate alone. Moreover, the increased stiffness didn’t prevent alginate-GO also from responding to external stimuli like alginate alone can. The researchers showed that by bathing the materials in a chemical that removes its ions, the materials swelled up and became much softer. The materials regained their stiffness when ions were restored through bathing in ionic salts. Experiments showed that the materials’ stiffness could be tuned over a factor of 500 by varying their external ionic environment.

That ability to change its stiffness could make alginate-GO useful in a variety of applications, the researchers say, including coatings.

Because alginate-GO retains the powerful oil-repellant properties of pure alginate, the new material could make an excellent coating to keep oil and other grime from building up on surfaces. In a series of experiments, the researchers showed that a coating of alginate-GO could keep oil from fouling the surface of glass in highly saline conditions. That could make alginate-GO hydrogels useful for coatings and structures used in marine settings, the researchers say.

“These composite materials could be used as a sensor in the ocean that can keep taking readings during an oil spill, or as an antifouling coating that helps to keep ship hulls clean,” Wong said. The extra stiffness afforded by the graphene would make such materials or coatings far more durable than alginate alone.

The researchers plan to continue experimenting with the new material, looking for ways to streamline its production and continue to optimize its properties.

Additional co-authors of the study include Alexander K. Landauer, Luke C. Morales, Eric M. DuBois, Shashank Shukla, Muchun Liu, and Lauren H. Stephens of Brown University, as well as Christian Franck of the University of Wisconsin, and Po-Yen Chen of the National University of Singapore. The research was supported by the U.S. Department of Education’s GAANN Training Grant in Applications and Implications of Nanotechnology, (P200A150037), the National Science Foundation (DGE-1058262) and a Brown University Hibbitt Postdoctoral Fellowship.