www.pcimag.com/articles/105248-self-crosslinking-resin-from-the-lubrizol-corp

Self-Crosslinking Resin from The Lubrizol Corp.
September 1, 2018
Aptalon™ W8062 is a waterborne, self-crosslinking resin providing resistance to hydrolysis, a broad assortment of chemicals and abrasion, while imparting very high hardness. A 1K dispersion, it meets or exceeds the performance properties of many 2K solventborne finishes without the need for external crosslinkers. Visit www.lubrizol.com.