BASF to Expand Capacity for Highly Chromatic Yellow Pigments
LUDWIGSHAFEN, Germany — BASF announced that the company plans to extend its production capacities for isoindoline yellow pigments by around 70% by 2020, as the demand for high-performance pigments grows. Bright yellow tones that offer a high degree of weather resistance and temperature stability are sought after, particularly in demanding applications involving industrial coatings.
“Following our recently announced expansion to production capacities for Paliocrom® effect pigments, this investment of around €10 million underscores our ambitions for growth as one of the leading manufacturers of high-performance pigments,” said Dr. Alexander Haunschild, Managing Director and Senior Vice President for BASF’s global pigments brand.
Customers use isoindoline pigments, marketed under the Colors & Effects® brand, to meet their steadily growing need for coatings for the automotive sector and to color plastics.