Gabriel Performance Products Buys Royce International

May 4, 2018

AKRON, OH — Gabriel Performance Products, a U.S.-based specialty chemicals company, announced the acquisition of Royce International.

Headquartered in Sarasota, Florida, Royce International is a custom solutions provider of specialty epoxy resins, diluents, curing agents and additives. These are sold under the RoyOxy™ trademark into CASE applications.

“The acquisition of Royce further expands Gabriel’s offerings of solutions for the coatings, adhesives and composites markets,” said Seth Tomasch, CEO of Gabriel. “Royce’s diversified product portfolio, technical support and formulation expertise will allow us to provide a broader array of products and services to our customers.”

Harry Anand, CEO of Royce, said, “Customers of both companies will be served well by this acquisition. Combined, the two companies will have a broader line of specialty products, technical expertise and manufacturing capabilities.”

Royce Associates, a sister company of Royce International, is not a part of this transaction and will continue to manufacture and supply its line of reductive chemicals, solvent and basic dyes, color concentrates, additives, and other specialty chemicals.