Tank Coating
A high-performance, chemical resistant, two-component epoxy coating, Hempadur 15600 is designed specifically for floating production storage and offloading (FPSO) cargo tank protection. The coating is compliant with the International Maritime Organization (IMO) Performance Standard for Protective Coatings (PSPC). It provides excellent resistance to continuous immersion in hydrocarbons, including crude oil up to 90˚C/194˚F.
Maurice Steijger, Group Offshore Manager, Hempel A/S, said, "Hempadur 15600 is an important part of Hempel's range of high-performance coatings for cargo tank protection within the offshore oil and gas industry. It offers the application benefits of a pure epoxy coating with the corrosion protection and temperature resistance of an epoxy phenolic coating. It is particularly suitable for FPSO contractors and owners specifying coatings for their cargo and slop tanks.
"Hempadur 15600 is mechanically robust and can be applied in just two coats to comfortably achieve the required dry film thickness for most cargo oil tank specifications. This enhanced performance is due to Hempel's high cross-link density technology, which gives added chemical and corrosion resistance and a hard, glossy surface for easy cleaning. Application costs and risks are reduced, and the coating offers resistance to hydrocarbons, including crude oil, at temperatures up to 90 ˚C/194 ˚F."
Additionally, this high temperature resistance ensures excellent performance at temperatures where conventional pure and modified epoxy universal primers can display limited resistance.
For shipyards, Hempadur 15600 delivers fast drying and curing properties resulting in a hard, smooth and easy clean surface; and after six hours it is re-coatable, saving further time and costs during dry-docking and maintenance. Unlike many other cargo tank coatings, Hempadur 15600 can be applied at temperatures as low as -5°/23 °F, offering more flexibility during winter working conditions.