Concrete Coating
CHEMLINE ARC adheres extremely well to concrete with the use of a primer. It is widely used in both the construction and contractor markets due to its excellent physical properties and resistance to moisture issues. Typical applications include secondary containment for oil and gas, wastewater basins, parking garages, foundations, and water ponds.
CHEMLINE ARC is a fast-set, spray applied, two-component polyurea that contains 100% solids and zero VOCs. It is a pure polyurea, meaning that it yields better chemical resistance and handles wider range of temperature fluctuations. It also offers superior corrosion protection and chemical resistance. CHEMLINE ARC will exhibit excellent impact resistance even in sub-freezing weather. With a 12-second gel time, it provides rapid turn around and reduces labor costs. Additionally, this product is certified to meet ANSI/NSF 61 standards for potable water by Underwriters Laboratory.
CHEMLINE ARC must be applied using a high-pressure, heated plural-component pump. Chemline recommends Graco Reactor E-XP1 or H-XP2 and is a top-20 Graco distributor.
Visit www.chemline.net.