The Computrac® Vapor Pro® XL is a chemical-free, moisture-specific alternative to Karl Fischer titration. It features an upgraded heater, which increases the upper limit for testing temperatures to 300 °C and allows for improved control over testing temperatures. It is compatible with multiple sizes of sample vials and is equipped with stepped temperature testing capabilities for enhanced method development. Visit www.azic.com/vpr.