K-POLĀ® 8211 Diol Modifier for 2K PU Systems
April 10, 2016
K-POL 8211is a unique, 100% active, aliphatic and saturated diol recommended for two-component polyurethane coatings, elastomers and coatings formulated with amino crosslinking resins. It provides hard films with good flexibility. K-POL 8211 will provide lower VOC systems with improved toughness, high modulus and good exterior durability, plus excellent performance in thin film coatings.
K-POL 8211 can be used in a variety of applications including industrial maintenance, automotive OEM/refinish, general industrial, urethane elastomers, adhesives and sealants.
- Higher Hardness
- Excellent Flexibility
- Improved Durability
- Higher Modulus