www.pcimag.com/articles/101875-hardener

Hardener
BASF
April 5, 2016
Used as an aminic hardener in epoxy resin systems, ÂBaxxodur® EC210, a cycloaliphatic diamine methylcyclohexyldiamine, improves coatings for industrial floors and bridges. Now available in commercial quantities, it is higher yielding, has lower viscosity, and can be processed longer than comparable products. Visit www.intermediates.basf.com.