RHOPLEX™ 800h acrylic binder, created to allow for early hardness development in low-VOC paints, employs hard, soft and functional monomers in a single waterborne acrylic binder to help improve hardness and block resistance in high-gloss and deep-tone architectural paints. Coatings formulated with RHOPLEX 800h binder show improved tack resistance and demonstrate excellent scrape and print resistance.

APEO-free and solvent-free, ROVACE™ 10 vinyl acrylic binder offers low-VOC technology for flat to semigloss interior paints. In formulated paints, ROVACE 10 emulsion has also undergone testing to show it can be formulated to meet MPI specifications #44, #53, and #143.