October 1, 2015
Developed to be free of solvents, surfactants and tin catalysts, CN9500 and CN9501 are supplied at approximately 40% solids content and are compatible with other water-based coatings. They contribute excellent coatings properties after water removal and UV curing, including good flow and leveling and a low minimum film formation temperature. Visit www.sartomer.com.