MIL-DTL-64159 Type III Chemical Agent Resistant Coating (CARC) Aerosol from Sherwin-Williams is now available for touch-ups or other small-job applications on military vehicles, ground support equipment and rotocraft. A specially designed aerosol can allows military personnel to mix the two-part coating through a simple procedure that includes shaking the can, depressing a plunger to mix the coating, and shaking once more prior to application, saving time and allowing rapid field recoating.

The water-reducible topcoat is Qualified Products Database (QPD) approved and is available in multiple CARC colors and is easily portable in 250mL and 400mL sizes. The topcoat combines superior corrosion resistance in a CARC coating.

Visit www.oem.sherwin.com.